Please use this identifier to cite or link to this item: https://idr.nitk.ac.in/jspui/handle/123456789/11063
Title: Evaluation of hydrogen-assisted cracking susceptibility in modified 9cr-1mo steel welds
Authors: Chakraborty, G.
Rejeesh, R.
Ramana, O.V.
Albert, S.K.
Issue Date: 2020
Citation: Welding in the World, 2020, Vol.64, 1, pp.115-122
Abstract: The hydrogen-assisted cracking susceptibility of modified 9Cr-1Mo steel weld is evaluated by Y-groove and gapped bead-on-plate test. It is found that a combination of pre + post heat is able to prevent cracking. However, the pre + post heat temperature combination determined from G-BOP test to prevent cracking (200 C) is found to be higher than that in Y-groove test (100 C). This is attributed to the higher weld restraint experienced in G-BOP than Y-groove test. For both the tests, the weld metal is found to be more susceptible to cracking than the heat affected zone. In addition to the diffusible hydrogen content of the welding consumables, diffusible hydrogen present in the G-BOP specimens prepared with different preheating and combinations of pre + post heat is also estimated by maintaining identical cooling conditions. The diffusible hydrogen in the weld for which no cracking is reported for G-BOP test (200 C pre + post heat) is less than 1 ml/100 g. Considering the high restraint conditions present in the G-BOP test, it can be concluded that to prevent HAC in P91 steel, the choice of welding parameters (hydrogen content in welding consumable, heat input, pre/post-heating) should be such that diffusible hydrogen in the weld is brought down to below 1 ml/100 g. 2019, International Institute of Welding.
URI: http://idr.nitk.ac.in/jspui/handle/123456789/11063
Appears in Collections:1. Journal Articles

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.