dc.description.abstractCompression testing of Ti-6Al-4V alloy has been carried out at temperatures between 303 K to 873 K. To prevent embrittlement due to atmospheric oxygen and nitrogen, the samples were given a glass coating, which also acts as a lubricant simultaneously. Dynamic Strain Aging was observed to occur in the temperature range of 600 K to 800 K. Below 600 K stresses were high. Warm working has to be done above 800 K but below 1163 K (0.6 Tm where Tm = 1940 K) which is the recrystallization temperature. Based on these conclusions, warm extrusion has been successfully carried out in the Materials Forming Laboratory of I.I.T., Madras, Chennai, India.en_US
dc.identifier.citationMaterials and Manufacturing Processes, 2008, Vol.23, 4, pp.342-346en_US
dc.identifier.urihttps://idr.nitk.ac.in/handle/123456789/10317
dc.titleCompression testing of Ti-6Al-4V in the temperature range of 303-873 Ken_US
dc.typeArticleen_US

Files

Original bundle

Now showing 1 - 1 of 1
Thumbnail Image
Name:
10317.pdf
Size:
936 KB
Format:
Adobe Portable Document Format