Compression testing of Ti-6Al-4V in the temperature range of 303-873 K

Thumbnail Image

Date

2008

Authors

Srinivasan, K.
Venugopal, P.

Journal Title

Journal ISSN

Volume Title

Publisher

Abstract

Compression testing of Ti-6Al-4V alloy has been carried out at temperatures between 303 K to 873 K. To prevent embrittlement due to atmospheric oxygen and nitrogen, the samples were given a glass coating, which also acts as a lubricant simultaneously. Dynamic Strain Aging was observed to occur in the temperature range of 600 K to 800 K. Below 600 K stresses were high. Warm working has to be done above 800 K but below 1163 K (0.6 Tm where Tm = 1940 K) which is the recrystallization temperature. Based on these conclusions, warm extrusion has been successfully carried out in the Materials Forming Laboratory of I.I.T., Madras, Chennai, India.

Description

Keywords

Citation

Materials and Manufacturing Processes, 2008, Vol.23, 4, pp.342-346