Creep cavitation damage of K-type thermocouples

dc.contributor.authorRakshan Kumar, J.K.
dc.contributor.authorBhattacharjee, D.
dc.contributor.authorDsilva, P.
dc.contributor.authorPraveen, R.
dc.contributor.authorHegde, S.R.
dc.date.accessioned2026-02-04T12:27:17Z
dc.date.issued2023
dc.description.abstractThis work investigates premature failure of K-Type thermocouples that were used in a chemical processing plant. The work presents a detailed metallurgical failure analysis involving, site visit, visual inspection, metallography, optical microscopy, scanning electron microscopy, and fractography. The analysis reveals that the thermocouple wires endured creep cavitation damage during service and eventually failed by creep-rupture. Interestingly, the influence of creep on the degradation of industrial thermocouples is not detected and reported thus far. By presenting analytical stress calculations using temperature dependent materials properties, the current work reveals that the thermal expansion mismatch between various materials of thermocouple causes high tensile stresses in the thermocouple wires during elevated temperature services. The work concludes that high tensile stresses at elevated temperature operation caused premature creep failure of the K-type thermocouples. © 2022
dc.identifier.citationEngineering Failure Analysis, 2023, 143, , pp. -
dc.identifier.issn13506307
dc.identifier.urihttps://doi.org/10.1016/j.engfailanal.2022.106846
dc.identifier.urihttps://idr.nitk.ac.in/handle/123456789/22202
dc.publisherElsevier Ltd
dc.subjectChemical industry
dc.subjectCreep
dc.subjectFracture mechanics
dc.subjectMetallography
dc.subjectMicrostructure
dc.subjectThermal expansion
dc.subjectThermocouples
dc.subjectWire
dc.subjectCavitation damage
dc.subjectChemical processing plants
dc.subjectCreep cavitation
dc.subjectElevated temperature
dc.subjectK-type thermocouples
dc.subjectMetallurgical failure analysis
dc.subjectPremature failures
dc.subjectSite visits
dc.subjectThermal expansion mismatch
dc.subjectThermocouple wires
dc.subjectScanning electron microscopy
dc.titleCreep cavitation damage of K-type thermocouples