Influence of combined grain refinement and modification on the microstructure, tensile strength and wear properties of Al-15Si, Al-15Si-4.5Cu alloys
No Thumbnail Available
Date
2015
Authors
Channappagoudar, S.
Sannayallappa, N.
Desai, V.
Karodi, V.
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
Microstructure, tensile strength and dry sliding wear studies of Al-15Si, Al-15Si-4.5Cu alloys with and without grain refinement and modifications are presented. Experimental alloys such as Al-15Si and Al-15Si-4.5Cu were conventionally melted and gravity die cast. For grain refinement, 1 wt.% of Al-1Ti-3B and for modification, 0.17 wt.% of aluminum phosphide (AlP) and 0.4 wt.% of Al-10Sr were added to the alloy melt. The results reveal refined microstructure due to grain refinement, modification, improved hardness, higher tensile strength and better sliding wear. Moreover, Al-15Si-4.5Cu alloy (untreated and treated) showed improved mechanical properties as compared to conventional hypereutectic Al-Si alloy. Carl Hanser Verlag GmbH & Co. KG.
Description
Keywords
Citation
International Journal of Materials Research, 2015, Vol.106, 8, pp.962-969