Influence of austenitising temperature on the formation of strain induced martensite in austempered ductile iron
| dc.contributor.author | Daber, S. | |
| dc.contributor.author | Ravishankar, K.S. | |
| dc.contributor.author | Prasad Rao, P.P. | |
| dc.date.accessioned | 2026-02-05T09:36:54Z | |
| dc.date.issued | 2008 | |
| dc.description.abstract | The present work was taken up to study the influence of austenitising temperature on the formation of strain-induced martensite in austempered ductile iron. Ductile iron containing 1.5 wt.% nickel, 0.3 wt.% molybdenum and 0.5 wt.% copper was subjected to austempering treatments which consisted of three austenitising temperatures, namely 850, 900 and 950 °C, and three austempering temperatures, namely 300, 350 and 400 °C. Tensile tests were carried out under all the heat-treatment conditions and strain-hardening behaviour was studied by applying Hollomon equation. Microstructures were studied by optical microscopy and X-ray diffraction. It was found that increasing austenitising temperature increased the tendency for the formation of strain-induced martensite at all the austempering temperatures. © 2008 Springer Science+Business Media, LLC. | |
| dc.identifier.citation | Journal of Materials Science, 2008, 43, 14, pp. 4929-4937 | |
| dc.identifier.issn | 222461 | |
| dc.identifier.uri | https://doi.org/10.1007/s10853-008-2717-8 | |
| dc.identifier.uri | https://idr.nitk.ac.in/handle/123456789/27726 | |
| dc.subject | Copper | |
| dc.subject | Ductility | |
| dc.subject | Imaging techniques | |
| dc.subject | Iron | |
| dc.subject | Lithography | |
| dc.subject | Martensite | |
| dc.subject | Microscopic examination | |
| dc.subject | Molybdenum | |
| dc.subject | Nickel | |
| dc.subject | Optical microscopy | |
| dc.subject | Tensile testing | |
| dc.subject | X ray analysis | |
| dc.subject | X ray diffraction analysis | |
| dc.subject | (O-sec.-butyldithiocarbonatio-S ,S') copper | |
| dc.subject | Austempered ductile iron (ADI) | |
| dc.subject | Austempering | |
| dc.subject | Business media | |
| dc.subject | Ductile iron | |
| dc.subject | Hollomon equation | |
| dc.subject | Optical (PET) (OPET) | |
| dc.subject | Reactivity (Chemical) | |
| dc.subject | special sections | |
| dc.subject | Springer (CO) | |
| dc.subject | Strain-hardening | |
| dc.subject | Strain-induced martensite | |
| dc.subject | Tensile tests | |
| dc.subject | Treatment conditions | |
| dc.subject | X ray diffraction (XRD) | |
| dc.subject | Temperature | |
| dc.title | Influence of austenitising temperature on the formation of strain induced martensite in austempered ductile iron |