Effect of simulated heating of plasma coating and ceramic firing on Ti and Ti-6Al-4V
| dc.contributor.author | Kotian, R. | |
| dc.contributor.author | Rao, P.P. | |
| dc.contributor.author | Bangera, M.K. | |
| dc.contributor.author | Madhyastha, P. | |
| dc.contributor.author | Srikant, S. | |
| dc.date.accessioned | 2026-02-05T09:29:44Z | |
| dc.date.issued | 2019 | |
| dc.description.abstract | The study was performed to understand the impact of heat in plasma coating and ceramic firing of titanium (Ti) and titanium alloy (Ti-6Al-4V) on their mechanical properties, and microstructure. Standard specimens were prepared to measure tensile strength before and after simulated heating cycles using Instron machine of model 4206 at a crosshead speed of 1â»mm/min. Yield strength, ultimate strength, and elongation were recorded. The microstructure was studied using an optical microscope. The mechanical properties, microstructure, and grain size remained the same as that of as-received samples at temperatures of 600 and 700â»°C for both Ti and Ti-6Al-4V. At temperature 800 and 900â»°C decrease in yield strength, and ultimate tensile strength with a change in microstructure was observed. The temperature of plasma coating and ceramic firing that Ti and Ti-6Al-4V metal substrates encounter during the fabrication of coated implants and metal-ceramic restorations do not affect the mechanical properties and microstructure. Above 800â»°C, a significant change in mechanical properties and microstructure is observed. © 2019 The Authors. | |
| dc.identifier.citation | Journal of Materials Research and Technology, 2019, 8, 5, pp. 4699-4704 | |
| dc.identifier.issn | 22387854 | |
| dc.identifier.uri | https://doi.org/10.1016/j.jmrt.2019.08.015 | |
| dc.identifier.uri | https://idr.nitk.ac.in/handle/123456789/24401 | |
| dc.publisher | Elsevier Editora Ltda | |
| dc.subject | Aluminum alloys | |
| dc.subject | Aluminum coatings | |
| dc.subject | Ceramic materials | |
| dc.subject | Heat treatment | |
| dc.subject | Microstructure | |
| dc.subject | Substrates | |
| dc.subject | Tensile strength | |
| dc.subject | Ternary alloys | |
| dc.subject | Titanium | |
| dc.subject | Yield stress | |
| dc.subject | Ceramic restorations | |
| dc.subject | Crosshead speed | |
| dc.subject | Metal substrate | |
| dc.subject | Properties and microstructures | |
| dc.subject | Standard specimens | |
| dc.subject | Ti-6 Al-4 V | |
| dc.subject | Ultimate strength | |
| dc.subject | Ultimate tensile strength | |
| dc.subject | Titanium alloys | |
| dc.title | Effect of simulated heating of plasma coating and ceramic firing on Ti and Ti-6Al-4V |