Durability studies of polypropylene fibre reinforced concrete

dc.contributor.authorSrikumar, R.
dc.contributor.authorDas, B.B.
dc.contributor.authorGoudar, S.K.
dc.date.accessioned2026-02-08T16:50:35Z
dc.date.issued2019
dc.description.abstractA research programme was initiated to understand the durability of polypropylene fibre reinforced concrete (PFRC). PFRC was prepared with varying dosages of polypropylene fibre. Dosages used were 0.5–1.5% of cement content (by weight) with an interval of 0.5% and was added as a cement replacement to concrete mix. Durability studies were carried out by exposing the 28 days cured cubical specimens into marine environment having different pH levels (1, 4, 7, 10 and 13). The varying pH levels represent the pH of industrial effluents. The marine environment was simulated in the laboratory by adding 3.5% NaCl to the tap water. The specimens were exposed for the durations of 60 and 90 days. The resistance of concrete to marine environment was measured through compressive strength retention and ultimate bond strength retention. Scanning Electron Microscopy (SEM) studies were also carried out to understand the fibre dispersion. Test results show that compressive and bond strength increases with increase in pH and decreases with increase in immersion duration. Concrete with 0.5 and 1% fibre content are more desirable and have given higher residual compressive and residual bond strength when compared to concrete with 1.5% fibre content. © Springer Nature Singapore Pte Ltd. 2019.
dc.identifier.citationLecture Notes in Civil Engineering, 2019, Vol.25, , p. 727-736
dc.identifier.isbn9789819620951
dc.identifier.isbn9783031951060
dc.identifier.isbn9783031976964
dc.identifier.isbn9783031976889
dc.identifier.isbn9789819679706
dc.identifier.isbn9789819677986
dc.identifier.isbn9783031951145
dc.identifier.isbn9789819685356
dc.identifier.isbn9789819674879
dc.identifier.isbn9789819688333
dc.identifier.issn23662557
dc.identifier.urihttps://doi.org/10.1016/j.conbuildmat.2025.141955
dc.identifier.urihttps://idr.nitk.ac.in/handle/123456789/33877
dc.publisherSpringer
dc.subjectCompressive strength retention
dc.subjectConcrete
dc.subjectDurability
dc.subjectFibres
dc.subjectUltimate bond strength retention
dc.titleDurability studies of polypropylene fibre reinforced concrete