Compression testing of Ti-6Al-4V in the temperature range of 303-873 K
| dc.contributor.author | Srinivasan, K. | |
| dc.contributor.author | Venugopal, P. | |
| dc.date.accessioned | 2026-02-05T09:36:55Z | |
| dc.date.issued | 2008 | |
| dc.description.abstract | Compression testing of Ti-6Al-4V alloy has been carried out at temperatures between 303 K to 873 K. To prevent embrittlement due to atmospheric oxygen and nitrogen, the samples were given a glass coating, which also acts as a lubricant simultaneously. Dynamic Strain Aging was observed to occur in the temperature range of 600 K to 800 K. Below 600 K stresses were high. Warm working has to be done above 800 K but below 1163 K (0.6 Tm where Tm = 1940 K) which is the recrystallization temperature. Based on these conclusions, warm extrusion has been successfully carried out in the Materials Forming Laboratory of I.I.T., Madras, Chennai, India. | |
| dc.identifier.citation | Materials and Manufacturing Processes, 2008, 23, 4, pp. 342-346 | |
| dc.identifier.issn | 10426914 | |
| dc.identifier.uri | https://doi.org/10.1080/10426910801937405 | |
| dc.identifier.uri | https://idr.nitk.ac.in/handle/123456789/27740 | |
| dc.subject | Compression testing | |
| dc.subject | Flow of fluids | |
| dc.subject | Oxygen | |
| dc.subject | Recrystallization (metallurgy) | |
| dc.subject | Strain hardening | |
| dc.subject | Stress analysis | |
| dc.subject | Temperature control | |
| dc.subject | Dynamic Strain Aging | |
| dc.subject | Flow properties | |
| dc.subject | Warm working | |
| dc.subject | Titanium alloys | |
| dc.title | Compression testing of Ti-6Al-4V in the temperature range of 303-873 K |