Investigation of Indium doped Se-Te bulk chalcogenide glasses for electrical switching and phase changing applications

dc.contributor.authorJoshi, S.
dc.contributor.authorRodney, J.D.
dc.contributor.authorJames, A.
dc.contributor.authorBehera, P.K.
dc.contributor.authorUdayashankar, N.K.
dc.date.accessioned2026-02-04T12:25:03Z
dc.date.issued2024
dc.description.abstractRecently, Metal-doped Se-Te chalcogenides have gained a lot of interest due to their unique capacity for electrical switching, which makes them desirable for electronic applications. This study examines the electrical switching characteristics of bulk Se<inf>86−x</inf>Te<inf>14</inf>In<inf>x</inf> (0 ≤ x ≤ 6) amorphous alloys produced by the conventional melt-mix-quench process. The samples with an Indium atomic percentage between 2 to 6 exhibited a remarkable transition from a highly resistive to a low resistive state when subjected to an electric field with a current of 1 mA, displaying quick and reversible switching behaviour. The threshold voltage (V<inf>th</inf>) significantly dropped from 410.6 V to 49.2 V with an increase in Indium concentration. Additionally, above the specific current threshold, these bulk glasses demonstrated memory-type switching, demonstrating their potential for data storage applications. To comprehend the trend of glass forming ability, thermal stability range and Hruby's glass stability parameters, with their compositional dependency, Differential Scanning Calorimetry (DSC) was utilized. The sample Se<inf>80</inf>Te<inf>14</inf>In<inf>6</inf> emerged to be the fastest phase-changing material, with a memory switching current threshold of I<inf>th</inf> = 1.3 mA and a threshold voltage value of 49.2 V. To study the formation of crystallites in Se-Te-In alloy, X-ray diffraction patterns of pristine glass and the annealed sample were examined. Furthermore, temperature-dependent conductivity investigations showed a sharp rise in conductivity once the process crystallization begins (T<inf>x</inf>), and also the threshold voltage (V<inf>th</inf>) of the samples decreased linearly with rising temperature. Overall, this study provides valuable insights into the electrical switching behaviour and thermal properties of Se-Te-In chalcogenide glasses, enhancing their suitability in electronic devices. © 2024 Elsevier B.V.
dc.identifier.citationJournal of Alloys and Compounds, 2024, 978, , pp. -
dc.identifier.issn9258388
dc.identifier.urihttps://doi.org/10.1016/j.jallcom.2024.173427
dc.identifier.urihttps://idr.nitk.ac.in/handle/123456789/21227
dc.publisherElsevier Ltd
dc.subjectActivation energy
dc.subjectAmorphous alloys
dc.subjectChalcogenides
dc.subjectDifferential scanning calorimetry
dc.subjectDigital storage
dc.subjectElectric fields
dc.subjectIndium
dc.subjectAtomic percentage
dc.subjectChalcogenide glass
dc.subjectCurrent thresholds
dc.subjectElectrical phasis
dc.subjectElectrical switching
dc.subjectElectronics applications
dc.subjectMetal-doped
dc.subjectPhase changing materials
dc.subjectSwitching behaviors
dc.subjectSwitching characteristics
dc.subjectThreshold voltage
dc.titleInvestigation of Indium doped Se-Te bulk chalcogenide glasses for electrical switching and phase changing applications