Flexural and fracture performance of fiber reinforced self compacting alkali activated concrete– A DOE approach

No Thumbnail Available

Date

2024

Journal Title

Journal ISSN

Volume Title

Publisher

Elsevier B.V.

Abstract

Owing to their much-reduced carbon footprint and lower embodied energy, compared to conventional Portland Cement (OPC-based) Concrete mixes, Alkali Activated Concrete (AAC) mixes represent a pivotal advancement towards achieving sustainability goals. The fracture properties were investigated using Three-Point Bending Tests (3-PBT) under the mode I failure mechanism. This study utilises Taguchi analysis to analyse and optimise Self-Compacting Alkali-Activated Concrete (SAAC), focusing mainly on its flexural strength and fracture characteristics. An L-16 orthogonal array of experiments with three input parameters − replacement of Blast Furnace Slag (BFS) with Fly ash (FA) (0 %, 30 %, 40 %, and 50 %), Steel Fibers (SF) volume content (0 %, 0.25 %, 0.5 % and 0.75 %) and Notch to Depth (a<inf>0</inf>/d) ratio (0.2,0.3,0.4 and 0.5), at four levels each, was adopted. The Work of Fracture Method (WFM) and Double K Fracture Criterion (DKFC) were utilised to determine the Fracture Energy (G<inf>F</inf>) and fracture toughness, respectively. The results obtained from all the sixteen mixes showed that the F0-S0.75-N0.5 mix demonstrated better values in several parameters, such as flexural strength of 7.82 MPa,K<inf>IC</inf>ini of 0.928 MPa√m, K<inf>IC</inf>uns of 6.99 MPa√m and K<inf>IC</inf>ini/ K<inf>IC</inf>uns of 0.133. A maximum G<inf>F</inf> of 2350 N/m was obtained with F50-S0.75-N0.2 mix. However, all the inferior values of these parameters were observed with F50-S0-N0.5 mix, which recorded a flexural strength of 4.90 MPa, K<inf>IC</inf>ini of 0.612 MPa√m,K<inf>IC</inf>uns of 1.16 MPa√m, K<inf>IC</inf>ini/ K<inf>IC</inf>uns of 0.528 and G<inf>F</inf> of 125 N/m. Through Taguchi analysis, the optimal combination for flexural strength was identified as FA 0 %, SF 0.75 %, and a<inf>0</inf>/d 0.5 and for both Initial Fracture Toughness (K<inf>IC</inf>ini) and Unstable Fracture Toughness (K<inf>IC</inf>uns) at FA 0 %, SF 0.75 % and a<inf>0</inf>/d 0.4. For both the ratio of initial to unstable fracture toughness (K<inf>IC</inf>ini/ K<inf>IC</inf>uns) and fracture energy (G<inf>F</inf>), the optimum combination was FA 0 %, SF 0.75 % and a<inf>0</inf>/d 0.2. Furthermore, the results indicate that FA significantly influences K<inf>IC</inf>ini, while SF predominantly affects all other parameters. The predictive performance of the regression equations demonstrates good agreement with experimental outcomes. © 2024 Elsevier Ltd

Description

Keywords

Bending strength, Bending tests, Carbon footprint, Compression testing, Concrete mixtures, Fiber reinforced concrete, Fracture energy, Fracture toughness, Mortar, Portland cement, Self compacting concrete, Strain rate, Alkali-activated concretes, Energy, Fiber reinforced self-compacting alkali-activated concrete, Fibre-reinforced, Fracture property, K IC, Optimisations, Self-compacting, Taguchi analysis, Unstable fracture, Blast furnaces

Citation

Theoretical and Applied Fracture Mechanics, 2024, 133, , pp. -

Collections

Endorsement

Review

Supplemented By

Referenced By