Effect of molybdenum on high-temperature tribological performance in HVOF sprayed of WC-based coatings on superni-76
| dc.contributor.author | Behera, N. | |
| dc.contributor.author | Sarmah, P. | |
| dc.contributor.author | Chandramouli, T.V. | |
| dc.contributor.author | Ramesh, M.R. | |
| dc.date.accessioned | 2026-02-03T13:19:48Z | |
| dc.date.issued | 2025 | |
| dc.description.abstract | This study examines the effects of Mo on the high-temperature wear and friction behavior of HVOF-sprayed 70%WC-Co/25%Mo/5%C and 70%WC-CrC-Ni/30%Mo coatings on Superni-76. The ball-on-disc tribometer wear tests were conducted at different temperatures (300°C and 600°C) and loads (10 and 30?N) against counter body Al<inf>2</inf>O<inf>3</inf> ball. Microstructures and phase formation were investigated using SEM/EDS and XRD. The characterization of coating microhardness, surface roughness, and coating density was examined. The 70%WC-Co/25%Mo/5%C coating showed lower surface roughness and higher microhardness values than the 70%WC-CrC-Ni/30%Mo coating. The wear rate of the substrate increases with an increase in temperature, whereas 70%WC-Co/25%Mo/5%C and 70%WC-CrC-Ni/30%Mo coatings decrease with temperature from 300°C to 600°C. The coefficient of friction of substrate and coating decreases with increasing temperatures. The worn surfaces of 70%WC-Co/25%Mo/5%C and 70%WC-CrC-Ni/30%Mo coating contain oxide phases (WO<inf>3</inf>, Cr<inf>2</inf>O<inf>5</inf>) and lubrication phases (M<inf>0.2</inf>W<inf>0.8</inf>O<inf>3</inf>, CoMoO<inf>4,</inf> and MoO<inf>3</inf>) at 600°C. These oxide phases reduced the coating wear rate and coefficient of friction at 600°C. The 70%WC-Co/25%Mo/5%C coating showed improved resistance to wear and lower friction coefficient than the substrate and 70%WC-CrC-Ni/30%Mo coating. At temperatures of 300°C, the main abrasive wear mechanism changes to oxidative wear when the temperature reaches 600°C for both coatings. © The Author(s) 2025. | |
| dc.identifier.citation | Tribology - Materials, Surfaces and Interfaces, 2025, 19, 2, pp. 97-110 | |
| dc.identifier.issn | 17515831 | |
| dc.identifier.uri | https://doi.org/10.1177/17515831251332401 | |
| dc.identifier.uri | https://idr.nitk.ac.in/handle/123456789/20244 | |
| dc.publisher | SAGE Publications Ltd | |
| dc.subject | Abrasion | |
| dc.subject | Abrasive coatings | |
| dc.subject | Fatigue testing | |
| dc.subject | Inorganic coatings | |
| dc.subject | Microhardness | |
| dc.subject | Nickel coatings | |
| dc.subject | Sprayed coatings | |
| dc.subject | Thermal fatigue | |
| dc.subject | Coefficient of frictions | |
| dc.subject | Effect of mo | |
| dc.subject | Friction behaviour | |
| dc.subject | High temperature wear behavior | |
| dc.subject | Highest temperature | |
| dc.subject | HVOF | |
| dc.subject | Mo coatings | |
| dc.subject | Oxide phasis | |
| dc.subject | Tribological performance | |
| dc.subject | Wear and friction | |
| dc.subject | Solid lubricants | |
| dc.title | Effect of molybdenum on high-temperature tribological performance in HVOF sprayed of WC-based coatings on superni-76 |