Metastable microstructures at the interface between AISI 321 steel and molten aluminum during hot-dip aluminizing
| dc.contributor.author | Huilgol, P. | |
| dc.contributor.author | Udupa, K.R. | |
| dc.contributor.author | Bhat, K.U. | |
| dc.date.accessioned | 2026-02-05T09:31:06Z | |
| dc.date.issued | 2018 | |
| dc.description.abstract | The microstructure at the interface between AISI 321 stainless steel and molten aluminum was investigated which occurs during the process of hot-dip aluminizing. Microstructural characterization was carried out by scanning electron microscopy, transmission electron microscopy and X-ray diffraction. The study revealed the formation of metastable FeAl<inf>m</inf> and multiple twinned Al<inf>13</inf>Fe<inf>4</inf> phases at the interface between steel and aluminum. Multiple twinned Al<inf>13</inf>Fe<inf>4</inf> phase exhibits pseudo tenfold electron diffraction pattern. Another metastable phase Al<inf>3</inf>(NiFe) with an orthorhombic structure was formed as one of the eutectic phase mixture in the solidified aluminum topcoat. The Al<inf>3</inf>(NiFe) phase in the eutectic shares crystallographic orientation relationship with the Al matrix. Metastable intermetallic phases are being reported for the first time during hot-dip aluminizing. © 2018 Elsevier B.V. | |
| dc.identifier.citation | Surface and Coatings Technology, 2018, 348, , pp. 22-30 | |
| dc.identifier.issn | 2578972 | |
| dc.identifier.uri | https://doi.org/10.1016/j.surfcoat.2018.05.013 | |
| dc.identifier.uri | https://idr.nitk.ac.in/handle/123456789/25043 | |
| dc.publisher | Elsevier B.V. | |
| dc.subject | Aluminum | |
| dc.subject | Aluminum alloys | |
| dc.subject | Aluminum coated steel | |
| dc.subject | Binary alloys | |
| dc.subject | Eutectics | |
| dc.subject | High resolution transmission electron microscopy | |
| dc.subject | Interfaces (materials) | |
| dc.subject | Intermetallics | |
| dc.subject | Metastable phases | |
| dc.subject | Microstructure | |
| dc.subject | Phase interfaces | |
| dc.subject | Scanning electron microscopy | |
| dc.subject | Stainless steel | |
| dc.subject | Transmission electron microscopy | |
| dc.subject | 321 Stainless Steel | |
| dc.subject | Crystallographic orientation relationships | |
| dc.subject | Hot dip aluminizing | |
| dc.subject | Intermetallic phasis | |
| dc.subject | Metastable microstructure | |
| dc.subject | Micro-structural characterization | |
| dc.subject | Orthorhombic structures | |
| dc.subject | Scanning electrons | |
| dc.subject | Austenitic stainless steel | |
| dc.title | Metastable microstructures at the interface between AISI 321 steel and molten aluminum during hot-dip aluminizing |