    Strength retention characteristics of concrete cubes subjected to elevated temperatures
    (2010) Yaragal, S.C.; Clarke, K.S.; Mahesh Babu, K.; Ashokumar, S.; Venkataramana, K.; Babu Narayan, K.S.; Chinnagiri Gowda, H.C.; Reddy, G.R.; Sharma, A.
    Concrete in structures is likely to be exposed to high temperatures during fire. The relative properties of concrete after such an exposure are of great importance in terms of the serviceability of buildings. The probability of its exposure to elevated temperatures is high due to natural hazards, accidents and sabotages. Therefore, the performance of concrete during and after exposure to elevated temperature is a subject of great interest to the designer. Physical changes like cracking, colour change, spalling and chemical changes like decomposition of Ca(OH)2 and the C-S-H gel take place when subjected to elevated temperatures. This work reports the characteristics of concrete at elevated temperatures. Popular normal strength grades (M20, M25, M30, M35, M40 and M45) produced by Ready Mix Concrete (RMC) India, Mangalore have been used in production of test specimens (150 mm cubes) to obtain more meaningful and realistic data. In the preliminary phase 150 mm cubes were cast, cured and tested by destructive method for gathering data on strength characteristics. Later these test samples were subjected to elevated temperatures ranging from 100°C to 800°C, in steps of 100°C with a retention period of 2 hours. After exposure, weight losses were determined and then again destructive tests were conducted to estimate the residual compressive strength. Test results indicated that weight and strength significantly reduces with an increase in temperature. © 2010 CAFET-INNOVA TECHNICAL SOCIETY.
  • Item
    Studies on normal strength concrete cubes subjected to elevated temperatures
    (2010) Yaragal, S.C.; Babu Narayan, K.S.; Venkataramana, K.; Kulkarni, K.S.; Gowda, H.C.C.; Reddy, G.R.; Sharma, A.
    Concrete in structures is likely to be exposed to high temperatures during fire. The probability of its exposure to elevated temperatures is high due to natural hazards, accidents and sabotages. Therefore, the performance of concrete during and after exposure to elevated temperature is a subject of great importance and interest to the designer. Popular normal strength grades of concrete produced by Ready Mix Concrete (RMC) India, Mangalore have been used in production of test specimens (150 mm cubes), cured and tested by destructive method for gathering data on strength characteristics. Later, these test samples were subjected to elevated temperatures ranging from 100 C to 800 C, in steps of 100 C with a retention period of 2 hours. After exposure, weight losses and the residual compressive strength retention characteristics are studied. Test results indicated that weight and strength significantly reduces with an increase in temperature. Residual compressive strength prediction equations are proposed for normal strength concretes subjected to elevated temperatures.
  • Item
    Effect of recuring on compressive strength of thermally deteriorated concrete cubes
    (2011) Prasanth, S.; Yaragal, S.C.; Babu Narayan, K.S.
    Concrete is found to undergo degradation when subjected to elevated temperatures during an event such as fire and lose substantial amount of its strength. The loss of strength in concrete is mainly attributed to decomposition of C-S-H and release of chemically bound water, which begins when the exposure temperature exceeds 500°C. When thermally deteriorated concrete is supplied with water there is a substantive gain in strength as a consequence of rehydration of cement that is initiated. This paper presents results of an experimental program carried out to investigate the effect of recuring on strength gain of normal strength concrete specimens subjected to elevated temperatures from 500°C to 800°C, which were subjected to retention time of two hours at the designated temperatures. © 2011 CAFET-INNOVA TECHNICAL SOCIETY. All rights reserved.
  • Item
    Core recovery: a damage diagnosis tool for thermally deteriorated concrete
    (Emerald Group Holdings Ltd., 2019) Kulkarni, K.S.; Yaragal, S.C.; S.k, B.N.
    Purpose: This paper aims to study and assess residual strengths of concrete specimen exposed to elevated temperatures by core recovery tests. Design/methodology/approach: The appraisal of concrete structures is typically carried out by means of partially destructive tests such as tests on concrete cores taken from the structure and non-destructive testing. Findings: This paper presents results associated with determination of residual compressive strengths of plain and reinforced concrete elements exposed to elevated temperatures by core recovery test. Physical observations and results of compressive strengths of cores extracted from plain cement concrete, as well as from reinforced concrete beam elements exposed to elevated temperatures, have been presented. Originality/value: The empirical relations have been proposed between standard cube and core extracted for compressive strength of concretes exposed to elevated temperatures are useful for damage diagnosis. © 2019, Emerald Publishing Limited.
  • Item
    Performance evaluation of cement mortar compositions at elevated temperatures
    (Associated Cement Companies Ltd., 2019) Yaragal, S.C.; Vivek, S.; Kumar, B.
    Natural river sand is becoming scarce day by day due to rapid growth in construction sector. There is need for alternatives to be used in place of river sand. The performance of alternatives to river sand at elevated temperatures is also important in the likely event of fire accidents. In this study, the effect of elevated temperatures on the compressive strength of mortars containing Crushed Rock Fines (CRF) and Lateritic Sand (LS) is investigated. Cement mortar cubes were cast for varied proportion of lateritic soil and quarry dust as fine aggregate. Lateritic content was varied from 25%-100%, and 50% quarry dust was adopted. After 28 days of water curing, specimens were exposed to temperatures of 200, 400, 600, and 800°C. At room temperature, the compressive strength decreases with increase in level of lateritic fine aggregate. The lateritic mortar mixes (50, 75, and 100%) have exhibited superior elevated temperature endurance characteristics at 400, 600, and 800°C when compared to control mix. Even the 25% laterized mortar has performed equally well as that of control mix. At elevated temperatures, CRF blended mix has performed very poorly. Mortar containing lateritic sand has potential for utilization in buildings and other structures, for better fire endurance in the likely event of fire accidents. © 2019 Associated Cement Companies Ltd.. All rights reserved.
  • Item
    Effect of elevated temperatures on ferrochrome ash based mortars
    (Associated Cement Companies Ltd., 2019) Kumar, B.; Yaragal, S.C.; Das, B.B.
    Due to boom in construction sector, large amount of Ordinary Portland Cement (OPC) is being consumed. Cement production is energy intensive and releases large amount of CO2 into atmosphere. Efforts are on to bring down cement consumption by the use of secondary cementitious materials. An attempt is made to study the influence of combined effect of various levels of ferrochrome ash (FCA) and lime, as replacement to OPC for different cement mortar mixtures at elevated temperatures. FCA replacement considered is in the range of 0% to 20% and along with 7% lime as replacement to cement. Compressive strength of cementitious materials is being an important parameter in the design of structures. The main objective of this work is to assess the residual compressive strengths at different levels of temperatures (200, 400, 600, and 800ºC) for a retention period of half an hour. Residual strengths of mortar mixtures produced, using FCA, have shown a good performance. Upto 20% FCA and 7% lime, mixture turns out to be a good elevated temperatures enduring material. This would increase the suggested application for environmental friendly materials. Important differences were seen in microstructural observations with scanning electron microscope (SEM) for various levels of FCA and lime incorporated mortars. © 2019, Associated Cement Companies Ltd. All rights reserved.
  • Item
    Multi-criteria optimization of fly ash and iron ore tailing based concretes subjected to elevated temperatures
    (Associated Cement Companies Ltd., 2019) Yaragal, S.C.; Babu Narayan, K.S.; Kumar, B.; Francis, J.G.
    Due to the rapid increase in concrete utilization all over the world, there is increased consumption of Ordinary Portland Cement (OPC), natural fine aggregate (NFA), and natural coarse aggregates. Increased use of OPC, is posing a serious threat due to excess CO2 emissions, and its production is highly energy intensive. On the other hand, extraction and processing stone-based fine and coarse aggregates too, is energy intensive, and the virgin resources are fast depleting. Therefore, for sustainable development, efforts are on all over the world to look for alternative materials in place of conventional ones. In this study, it is attempted to partly replace OPC with fly ash (FA) and partly replace NFA by iron ore tailings (IOT) in concretes. The performance of such concretes at ambient and elevated temperatures is also presented. Full factorial design of experiments was adopted with two control factors under three levels of replacement, i.e., FA (0, 15, and 30% by weight of OPC) and IOT (0, 50, and 100% by volume of NFA). Total nine concrete mixes were prepared and tested for their compressive strengths at room temperature, and residual compressive strengths when subjected to various levels of elevated temperatures (200, 400, 600, and 800°C), and cost of these concretes has also been analyzed. Further, three traditional multi–criteria optimization methods, i.e., grey relational analysis (GRA), technique for order of preference by similarity to ideal solution (TOPSIS), and desirability function approach (DFA) were used to optimize concrete mixes. Results showed that TOPSIS based optimization method is more significant when compared to other two methods. Further, FA-based concrete mixes showed improved performance under multi-criteria optimization. © 2019, Associated Cement Companies Ltd. All rights reserved.
  • Item
    Effect of Elevated Temperatures on Sugarcane Bagasse Ash-Based Alkali-Activated Slag Concrete
    (Springer, 2021) Kumar, D.S.S.; Chethan, K.; Kumar, B.C.
    The main focus of researchers in construction sector is to check suitability of ecofriendly alternative materials. Sugarcane bagasse ash (BA) and steel slag (SS) is one among such ecofriendly alternative materials. BA and SS has potential to utilize as binder and coarse aggregate, respectively, in concrete production. In the present investigation, BA and SS were utilized in alkali-activated slag/bagasse ash concrete (AASBC) mixture production. Full factorial experimental design was considered with two input variables, i.e., BA (0, 25, and 50%) and SS (0, 50, and 100%) as replacement to ground granulated blast furnace slag and natural coarse aggregate, respectively. Effect of elevated temperatures on BA and SS-based AASBC mixture were examined. Field emission scanning electron microscope study were carried out to check the morphological changes in ambient and elevated temperature condition. In order to rank different BA and SS-based AASBC mixture performance multi-criteria optimization techniques like, grey relational analysis, technique for order preference by similarity to ideal solution, and desirability function approach were utilized. AASBC mixture with 25% BA content and 100% SS content found to be most suitable AASBC mixture based on multi-criteria optimization technique under elevated temperature conditions. © 2020, Society for Sugar Research & Promotion.
  • Item
    Numerical and experimental studies on sustainable alkali activated concretes at elevated temperatures
    (Emerald Publishing, 2023) Yaragal, S.C.; Kumar, B.; Abhinav, M.U.
    Purpose: To reduce environmental impact caused by excessive use of ordinary Portland cement (OPC) and to mitigate scarcity of base materials such as natural coarse aggregate (NCA), industrial by-products can be carefully used as alternatives to OPC and NCA, in production of concrete. This paper aims to describe the performance of using ground granulated blast furnace slag (GGBS), fly ash (FA) as a complete replacement to OPC and ferrochrome slag (FCS) as replacement to NCA in production of novel FCS based alkali activated slag/fly ash concretes (AASFC) and evaluate their performance at elevated temperatures. Design/methodology/approach: Two control factors with three levels each i.e. FA (0, 25 and 50 per cent by weight) and FCS (0, 50 and 100 per cent by volume) as a GGBS and NCA replacement, respectively, were adopted in AASFC mixtures. Further, AASFC mixture specimens were subjected to different levels of elevated temperature, i.e. 200°C, 400°C, 600°C and 800°C. Compressive strength and residual compressive strength were considered as responses. Three different optimization techniques i.e. gray relational analysis, technique for order preference by similarity to ideal solution and Desirability function approach were used to optimize AASFC mixtures subjected to elevated temperatures. Findings: As FA replacement increases in FCS based AASFC mixtures, workability increases and compressive strength decreases. The introduction of FCS as replacement to NCA in AASFC mixture did not show any significant change in compressive strength under ambient condition. AASFC produced with 75 per cent GGBS, 25 per cent FA and 100 per cent FCS was found to have excellent elevated temperature enduring properties among all other AASFC mixtures studied. Originality/value: Although several studies are available on using GGBS, FA and FCS in production of OPC-based concretes, present study reports the performance of novel FCS based AASFC mixtures subjected to elevated temperatures. Further, GGBS, FA and FCS used in the present investigation significantly reduces CO2 emission and environmental degradation associated with OPC production and NCA extraction, respectively. © 2019, Emerald Publishing Limited.