Faculty Publications

Permanent URI for this communityhttps://idr.nitk.ac.in/handle/123456789/18736

Publications by NITK Faculty

Browse

Search Results

Now showing 1 - 5 of 5
  • Item
    Effect of grain refinement on the performance of AZ80 Mg alloys during wear and corrosion
    (Techno-Press info@techno-press.com, 2018) Naik, G.M.; Gote, G.D.; Narendranath, S.; Satheesh Kumar, S.S.
    Magnesium and its alloys are attracted towards all engineering applications like automotive, marine, aerospace etc. due to its inherent high strength to weight ratio. But, extensive use of Mg alloys is limited to the current scenario because of low wear and corrosion resistance behavior. However, equal channel angular press is one of the severe plastic deformation technique which has been effective method to improve the wear and corrosion resistance by achieving fine grain structure. In this study, the effect of grain refinement on wear and corrosion resistance of AZ80 Mg alloys were investigated. The wear behavior of the coarse and fine-grained Mg alloys was examined through L9 orthogonal array experiments in order to comprehend the wear behavior under varies control parameters. It was shown that ECAPed alloy increased the wear and corrosion resistance of the Mg alloy through the formation of fine grain and uniform distribution of secondary beta - phase. Also, the performance of AZ80 Mg alloy for these changes was discussed through SEM morphology. © 2018 Techno-Press, Ltd.
  • Item
    Effect of grain refinement on material properties of Mg-8%Al-0.5%Zn alloy after the combined processes of multi-direction forging and equal channel angular pressing
    (Institute of Physics, 2019) Naik, G.M.; Anjan, B.N.; Narendranath, S.; S Satheesh Kumar, S.; Preetham Kumar, G.V.
    Establishing the novel microstructure is an effective method to accelerate the applications of magnesium and its alloys. In this work, an Mg-8%Al-0.5%Zn alloy (AZ80 Mg) with ultra-fine-grain (UFG) size of ?1.29 ?m was achieved by the combined processes of multi-directional forging (MDF) and equal channel angular pressing (ECAP). The achieved ultra-fine grain structure made the Mg alloy, owing to inclusive performance as the structural material. The AZ80 Mg alloy with MDF 6 pass followed by two pass ECAP has superior mechanical properties such as ultimate tensile strength (UTS) of 352 MPa and elongation of 11% when compared to as-received Mg alloy. Also, an unprocessed Mg alloy showed the corrosion rate of a 13.28 mm y?1, the corrosion rate of processed Mg alloy could be further decelerated through a change of microstructure obtained from combined processes of MDF and ECAP. This study outstandingly obtained a 94% reduction of corrosion rate after MDF-3P followed by an ECAP-2P (0.77 mm y?1) process compared to as-received Mg alloy. © 2019 IOP Publishing Ltd.
  • Item
    Bio-corrosion impacts on mechanical integrity of ZM21 Mg for orthopaedic implant application processed by equal channel angular pressing
    (Springer, 2021) Sekar, P.; Nyahale, M.B.; Naik, G.M.; Narendranath, N.; Prabhu, A.; Rekha, P.D.
    The mechanical integrity of rolled ZM21 Mg was improved by equal channel angular pressing (ECAP) to function as a potential biodegradable bone screw implant. Electron backscattered diffraction (EBSD) revealed deformed grains of 45 µm observed in rolled ZM21 Mg. They were transformed to equiaxed fine grains of 5.4 µm after 4th pass ECAP. The yield strength of rolled and ECAPed ZM21 Mg alloys were comparable. In contrast, 4th pass ZM21 Mg exhibited relatively higher elongation when compared to rolled sample. The mechanical properties of rolled and ECAPed ZM21 Mg were dependant on both grain refinement and crystallographic texture. The rolled and 4th pass ECAPed tensile samples exhibited nonlinear deterioration of mechanical properties when tested after 7, 14, 21 and 28 days immersion in Hank’s solution. The evaluation signifies that regardless their processing condition, ZM21 Mg alloys are suitable for surgical areas that requires high mechanical strength. In addition, the 4th pass ECAP samples were viable to MG-63 cells proving themselves to be promising candidates for future in vivo studies. [Figure not available: see fulltext.] © 2021, The Author(s).
  • Item
    Investigation of Tribological Characteristics of Cu-Ti Alloys Processed by Multi-Axial Cryo-Forging
    (Springer, 2022) Ramesh, S.; Shivananda Nayaka, H.S.; Anne, G.; Arun, M.N.; Naik, G.M.
    Cu-XTi alloys (X = 1.5 and 4.5%) were subjected to multi-axial forging (MAF) under cryogenic condition up to three passes successfully. Characteristics of the MAF-processed alloys were analyzed using microstructural analysis, hardness and wear tests. Worn surface morphology and elemental analysis was performed by scanning electron microscopy. The hardness of samples increases with higher MAF passes due to strain hardening and grain refinement. Wear test was done for six various sliding distances (500, 1000, 1500, 2000, 2500 and 3000 m), two different loads (10 and 20 N), and two different velocities (1 and 2 m/s) using the pin-on-disk wear test rig. Wear loss of as-received samples is higher than MAF-pressed samples due to an increase in hardness, but wear loss increases as the load increases. Coefficient of friction is reduced with the increase in MAF pass, which is due to strain hardening effect. The worn surface exhibits the plastic deformation regions, delamination, plowing and formation of oxide layers, which was revealed by energy-dispersive X-ray spectroscopy analysis. Also, MAF-processed samples exhibited abrasive wear mechanism as a result of formation of oxygen layer as revealed in SEM micrographs. © 2022, ASM International.
  • Item
    Enhancing surface characteristics of Mg-Zn-Sr alloy through cryo-ball burnishing; modeling and experimentation
    (Korean Society of Mechanical Engineers, 2024) Kudva, S.A.; Anne, G.; Ramesh, S.; Sharma, P.; Jagadeesh, C.; Ritti, L.; Naik, G.M.; Divya Deepak, G.D.
    In this investigation, the impact of the cryo-ball burnishing process on both the mechanical and corrosion properties of the Mg-4Zn-1Sr alloy was systematically explored. To better understand the plastic deformation occurring in Mg-4Zn-1Sr during cryo-burnishing, a finite element analysis (FEA) model was developed. The microstructure of cryo-ball burnished samples underwent characterization through scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray diffractometry (XRD), and surface properties were assessed using atomic force microscopy (AFM). Additionally, electrochemical impedance spectroscopy and potentiodynamic polarization tests were conducted in a simulated body fluid using an electrochemical workstation. Experimental findings revealed significant grain refinement and the presence of residual dislocations during the cryo-burnishing process, as evident in TEM analysis. XRD analysis indicated the presence of Mg, Mg17Sr2 and SrZn2 phases, with observable peak broadening in the cryo-burnished samples, attributed to structural refinement and lattice strain incorporation. Microhardness values increased with greater depth of press, with the DFN 1071 sample displaying a hardness of 80 ± 4 Hv (Ra = 1.853 µm), marking a 54 % improvement compared to the homogenized sample. The enhanced corrosion resistance of the Mg-4Zn-1Sr alloy due to cryo-burnishing is attributed to the combined effects of grain refinement, residual dislocations, and intermetallic phases. © The Korean Society of Mechanical Engineers and Springer-Verlag GmbH Germany, part of Springer Nature 2024.