Faculty Publications
Permanent URI for this communityhttps://idr.nitk.ac.in/handle/123456789/18736
Publications by NITK Faculty
Browse
27 results
Search Results
Item Dynamic impact resistance of composite sandwich panels with 3-D printed polymer syntactic foam cores(DEStech Publications, 2021) Tewani, H.R.; Bonthu, D.; Bharath, H.S.; Doddamani, M.; Prabhakar, P.Polymer-based syntactic foams find use in the marine industry as primary structural materials due to their inherent lightweight nature and enhanced mechanical properties relative to pure HDPE. 3-D printing these materials circumvents the use of joining assemblies, enabling the production of complex shapes as standalone structures. Although the quasi-static response of these 3D printed foams has been well studied independently in recent years, their dynamic impact resistance and tolerance as potential core material for sandwich panels have not been the focus. Moreover, 3D printing is known to impart directionality in the printed syntactic foams, which may introduce failure mechanisms typically not observed in molded foams. It is therefore important to investigate the mechanics of 3-D printed syntactic foam core composite sandwich structures under impact loading and characterize their failure mechanisms for establishing dynamic impact resistance. To this end, 3-D printed syntactic foams have been developed using rasters of High-Density Polyethylene (HDPE) and Glass MicroBalloon (GMB) fillers by adopting the Fused Raster Fabrication (FFF) technique. The current study is performed to assess the impact performance of these composite foam cores based on the volume fraction of fillers and print orientation. The weight percentage of GMB fillers in printed specimens ranges from 0% to 60% in increments of 20%. This study presents the impact response of these composite sandwich panels at different energy levels, in compliance with ASTM D7136/D7136M - 20. Observations suggest that an increase in GMB % in HDPE matrix improves the impact performance in terms of the peak load of the material, but the failure behavior becomes brittle to an extent. Observing the failed specimens under a Micro-CT scanner captures the failure morphologies and helps characterize failure processes during impact. It is noticed that core materials with higher GMB content are prone to individual raster breakage and delamination at the back face, in addition to debonding between individual rasters. Specimens printed along the longer dimension (y-direction) impart more warping in the final sandwich structures than that of specimens printed along the shorter dimension (x-direction). Therefore, they are more susceptible to delamination at the back face. Addition of GMB fillers mitigate the tendency of the sandwich panels to warp. © 2021 36th Technical Conference of the American Society for Composites 2021: Composites Ingenuity Taking on Challenges in Environment-Energy-Economy, ASC 2021. All Rights Reserved.Item Mechanical behavior of 3D printed syntactic foam composites(Elsevier Ltd, 2020) Bharath, H.S.; Sawardekar, A.; Waddar, S.; Jeyaraj, J.; Doddamani, M.A three-dimensional printed (3DP), polymer based syntactic foams are developed using hollow glass micro balloons (GMB) dispersed in high density polyethylene (HDPE). This work presents the buckling and vibration response of 3D printed foams subjected to axial compression. The buckling load is estimated using Modified Budiansky Criteria (MBC) and Double Tangent Method (DTM) through the load–deflection plots. The first three natural frequencies and their mode shapes are computed as a function of axial compressive load. It is noted that the natural frequency reduces with an increase in axial compressive load. It is also observed that with an increase in GMB %, the natural frequencies and critical buckling load increases. In mode-1, the natural frequency decreases in pre-buckling regimes and increases exponentially in post-critical loading conditions. Analytical solutions obtained from the Euler-Bernoulli-beam theory are compared with experimental results. It is noted that the fundamental frequency approaches zero when the axial load is equal to the critical load. The critical buckling load is estimated through the vibration correlation technique and compared with the results obtained using DTM and MBC methods. The property map is plotted for buckling load against the density of various composites. © 2020 Elsevier LtdItem Dry sliding wear of epoxy/cenosphere syntactic foams(Elsevier Ltd, 2015) Manakari, V.; Parande, G.; Doddamani, M.; Gaitonde, V.N.; Siddhalingeshwar, I.G.; Kishore; Shunmugasamy, V.C.; Gupta, N.Abstract Dry sliding wear behavior of epoxy matrix syntactic foams filled with 20, 40 and 60 wt% fly ash cenosphere is reported based on response surface methodology. Empirical models are constructed and validated based on analysis of variance. Results show that syntactic foams have higher wear resistance than the matrix resin. Among the parameters studied, the applied normal load (F) had a prominent effect on wear rate, specific wear rate (ws) and coefficient of friction (?). With increasing F, the wear rate increased, whereas ws and ? decreased. With increase in filler content, the wear rate and ws decreased, while the ? increased. With increase in sliding velocity as well as sliding distance, the wear rate and ws show decreasing trends. Microscopy revealed broken cenospheres forming debris and extensive deformation marks on the wear surface. © 2015 Elsevier Ltd.Item Enhancing the ignition, hardness and compressive response of magnesium by reinforcing with hollow glass microballoons(MDPI AG Postfach Basel CH-4005, 2017) Manakari, V.; Parande, G.; Doddamani, M.; Gupta, M.Magnesium (Mg)/glass microballoons (GMB) metal matrix syntactic foams (1.47-1.67 g/cc) were synthesized using a disintegrated melt deposition (DMD) processing route. Such syntactic foams are of great interest to the scientific community as potential candidate materials for the ever-changing demands in automotive, aerospace, and marine sectors. The synthesized composites were evaluated for their microstructural, thermal, and compressive properties. Results showed that microhardness and the dimensional stability of pure Mg increased with increasing GMB content. The ignition response of these foams was enhanced by -22 °C with a 25 wt % GMB addition to the Mg matrix. The authors of this work propose a new parameter, ignition factor, to quantify the superior ignition performance that the developed Mg foams exhibit. The room temperature compressive strengths of pure Mg increased with the addition of GMB particles, with Mg-25 wt % GMB exhibiting the maximum compressive yield strength (CYS) of 161 MPa and an ultimate compressive strength (UCS) of 232 MPa for a GMB addition of 5 wt % in Mg. A maximum failure strain of 37.7% was realized in Mg-25 wt % GMB foam. The addition of GMB particles significantly enhanced the energy absorption by -200% prior to compressive failure for highest filler loading, as compared to pure Mg. Finally, microstructural changes in Mg owing to the presence of hollow GMB particles were elaborately discussed. © 2017 by the authors. Licensee MDPI, Basel, Switzerland.Item Development of glass microballoon/HDPE syntactic foams by compression molding(Elsevier Ltd, 2017) Jayavardhan, M.L.; Bharath Kumar, B.R.; Doddamani, M.; Singh, A.K.; Zeltmann, S.E.; Gupta, N.Thermoplastic resins are widely used in consumer products and industrial components. There is a significant interest in weight reduction of many of those components. Although glass hollow particle filled lightweight syntactic foams with thermoset matrices have been studied in detail, studies on thermoplastic syntactic foams are scarce. The present study is focused on developing a compression molding based processing method for glass microballoon/high density polyethylene (GMB/HDPE) syntactic foams and studying their mechanical properties to develop structure-property correlations. Blending of GMB in HDPE is carried out using a Brabender mixer with processing parameters optimized for minimal filler breakage. Flexural and tensile test specimens are compression molded with 20, 40 and 60 vol% of GMB. Particle fracture increases with increasing GMB content due to increased particle to particle interaction during processing. Additionally, increasing wall thickness makes GMBs stronger and results in reduced particle fracture. Flexural modulus increases while strength decreases with increasing filler content. Tensile strength decreases with increasing filler content, while tensile modulus is relatively unchanged. GMB volume fraction has a more prominent effect than the wall thickness on the mechanical properties of syntactic foams. Specific moduli of GMB/HDPE foams are superior while specific strength is comparable to neat HDPE. © 2017 Elsevier LtdItem Compressive behavior of cenosphere/epoxy syntactic foams in arctic conditions(Elsevier Ltd, 2018) Shahapurkar, K.; Garcia, C.D.; Doddamani, M.; Mohan Kumar, G.C.; Prabhakar, P.In this paper, the effects of arctic condition on the compressive response of ceno-sphere/epoxy syntactic foams are investigated. Understanding the behavior of such foams under extreme conditions is critical for exploring their suitability for constructing lightweight platforms used in arctic explorations, which are exposed to subzero temperatures for extended periods of time potentially degrading their mechanical properties. In the research study presented here, samples of cenosphere/epoxy syntactic foams were conditioned under arctic environment at a temperature of ?60 °C for a period of 57 days. Compression tests were then conducted at room temperature as well as in-situ ?60 °C on the conditioned samples and compared against unconditioned samples tested at room temperature. Combinations of surface modification and cenosphere volume fractions were considered. For the case of unconditioned samples, compressive strength decreased with increasing cenosphere volume fraction for both surface modified and unmodified cenospheres. For the arctic conditioned samples, cenospheres/epoxy foams did not present visible signs of degradation prior to testing, but manifested a reduction in compressive modulus in a range of 47–57% and 47–65% for untreated and treated cenospheres/epoxy syntactic foams as compared to their unconditioned counterparts. On the other hand, the compressive strength increased in a range between 32–68% for untreated and 59–80% for treated cenosphere foams in arctic environment, which can be attributed to the matrix hardening introduced by frigid in-situ environment. Also, under in-situ arctic compressive loading, the post peak response for all foam types have shifted from a progressive failure to a brittle type behavior. © 2017 Elsevier LtdItem Influence of axial compressive loads on buckling and free vibration response of surface-modified fly ash cenosphere/epoxy syntactic foams(SAGE Publications Ltd info@sagepub.co.uk, 2018) Waddar, S.; Jeyaraj, P.; Doddamani, M.This work deals with experimental buckling and free vibration behavior of silane-treated cenosphere/epoxy syntactic foams subjected to axial compression. Critical buckling loads are computed from compressive load–deflection plots deduced using universal testing machine. Further, compressive loads are applied in the fixed intervals until critical loading point on different set of samples having similar filler loadings to estimate natural frequency associated with the first three transverse bending modes. Increasing filler content increases critical buckling load and natural frequency of syntactic foam composites. Increasing axial compressive load reduce structural stiffness of all the samples under investigation. Syntactic foams registered higher stiffness compared to neat epoxy for all the test loads. Similar observations are noted in case of untreated cenosphere/epoxy foam composites. Silane-modified cenosphere embedded in epoxy matrix registered superior performance (rise in critical buckling load and natural frequencies to the tune of 23.75% and 11.46%, respectively) as compared to untreated ones. Experimental results are compared with the analytical solutions that are derived based on Euler–Bernoulli hypothesis and results are found to be in good agreement. Finally, property map of buckling load as a function of density is presented by extracting values from the available literature. © The Author(s) 2018.Item Snap-through buckling of fly ash cenosphere/epoxy syntactic foams under thermal environment(Elsevier Ltd, 2018) Waddar, S.; Jeyaraj, P.; Doddamani, M.Experimental investigation on deflection behaviour of fly ash cenosphere/epoxy syntactic foam at room temperature and under thermal environment (three different heating conditions) is investigated. Influence of fly ash cenosphere volume fraction and nature of temperature variation on deflection behaviour of syntactic foam beam is discussed elaborately. Results reveal that the syntactic foam beam experience snap-through buckling under thermal environment and is reflected by two bifurcation points in temperature-deflection plot. It is observed that the time duration for which the foam beam stays in the first buckled position increases with increase in cenosphere content. Thermal environment induces compressive stresses in the samples causing such snap-through buckling. However, such phenomenon is not observed when mechanical compressive loads are applied under room temperature conditions. Temperature variation across the beam strongly influences snap-through buckling in syntactic foams in addition to volume fraction of filler content. © 2018 Elsevier LtdItem Quasi-static compressive response of compression molded glass microballoon/HDPE syntactic foam(Elsevier Ltd, 2018) Jayavardhan, M.L.; Doddamani, M.Quasi-static compressive behavior of different density glass microballoon (GMB) reinforced high density polyethylene (HDPE) syntactic foams are investigated in the present work. Reducing the weight of thermoplastic components has been always a high priority in transportation, aerospace, consumer products and underwater vehicle structures. Despite continued interest in developing lightweight thermoplastic syntactic foams, they have not been studied extensively for quasi-static response with focus on wall thickness and volume fraction variations. Compression molded GMB/HDPE sheets are subjected to 0.001, 0.01 and 0.1 s?1 strain rates. Compressive modulus of foams is higher compared to neat HDPE. Increasing strain rates and decreasing filler content increases yield strength for all the foams investigated compared to neat HDPE. Yield strain and energy absorption of GMB/HDPE foams increases with an increasing strain rate and wall thickness. Specific modulus and strength of GMB/HDPE foams are superior and are comparable to neat HDPE. GMB/HDPE foam achieved high stiffness to weight ratio making them suitable for wide variety of applications. Theoretical model based on differential scheme predicts a good estimate of elastic modulus for all the type of GMB/HDPE foams. Finally, property map is exhibited to present comparative studies with existing literature. © 2018 Elsevier LtdItem Effect of arctic environment on flexural behavior of fly ash cenosphere reinforced epoxy syntactic foams(Elsevier Ltd, 2018) Garcia, C.D.; Shahapurkar, K.; Doddamani, M.; Mohan Kumar, G.C.M.; Prabhakar, P.In this paper, the effect of arctic conditions on the flexural response of cenosphere/epoxy syntactic foams is investigated. Understanding the behavior of such foams under extreme conditions is critical for exploring their suitability for constructing lightweight platforms used in arctic explorations. Such platforms are exposed to subzero temperatures for extended periods of time potentially degrading their mechanical properties. In the research study presented here, samples of cenosphere/epoxy syntactic foams were conditioned under arctic environment at ?60 °C temperature for a period of 57 days. Flexural tests were then conducted at room temperature as well as in-situ ?60 °C on the conditioned samples and compared against unconditioned samples. Combinations of surface modification and cenosphere volume fractions were considered. Experimental findings showed that an increase in flexural modulus can be observed at room temperature with increasing cenosphere volume content for both untreated and treated cenosphere reinforced syntactic foams. In contrast, a decrease in flexural strength was observed as compared to neat resin. For the case of arctic exposed samples, an apparent increase in flexural modulus was recorded between 7-15% as compared to room temperature cenospheres/epoxy syntactic foams. In addition, an apparent increase of 3–80% in the flexural strength was observed under arctic environment. The conditioning of cenosphere/epoxy syntactic foams under low temperatures manifested lower strains to failure as compared to neat epoxy and they exhibit quasi-brittle behavior leading to sudden failure in the post peak regime. © 2018 Elsevier Ltd
- «
- 1 (current)
- 2
- 3
- »