    High-Temperature Erosive Behavior of Plasma Sprayed Cr3C2-NiCr/Cenosphere Coating
    (Springer New York LLC barbara.b.bertram@gsk.com, 2018) Mathapati, M.; Doddamani, M.; Ramesh, M.R.
    This research examines the deposition of Cr3C2-NiCr/cenosphere and Cr3C2-NiCr coatings on MDN 321 steel through the process of plasma spray. In this process, the solid particle erosion test is established at 200, 400, 600 °C with 30° and 90° impact angles. Alumina erodent is adopted to investigate the erosive behavior of the coating at higher temperatures. The properties of the Cr3C2-NiCr/cenosphere coating are established based on the microhardness, the adhesive strength, the fracture toughness, and the ductility. To quantify volume loss as a result of erosion, an optical profilometer is used. At higher temperature, decrease in the erosion volume loss of Cr3C2-NiCr/cenosphere and Cr3C2-NiCr coatings is observed. The erosion-resistive property of Cr3C2-NiCr/cenosphere coating is higher than that of MDN 321 steel by 76%. This property is influenced by high-temperature stability of mullite, alumina, and protective oxide layer that is formed at elevated temperatures. The morphology of eroded coating discloses a brittle mode of material removal. © 2018, ASM International.
  • Item
    Microstructure and tribological behavior of plasma sprayed NiCrAlY/WC-Co/cenosphere/solid lubricants composite coatings
    (Elsevier B.V., 2018) Doddamani, M.; Mathapati, M.; Ramesh, M.R.
    Present investigation deal with NiCrAlY/WC-Co/Cenosphere/MoS2/CaF2, NiCrAlY/WC-Co/Cenosphere/MoS2/CaSO4 and NiCrAlY/WC-Co/Cenosphere coatings deposited on MDN 321 steel using atmospheric plasma spraying. Tribological properties of MDN 321 steel and coatings are evaluated from room temperature (RT) to 600 °C under dry lubrication conditions using a pin on disc high-temperature tribometer. Scanning Electron Microscopy (SEM), X-ray diffraction (XRD) and Energy Dispersive Spectroscopy (EDS) are used to characterize the coatings. Presence of cenospheres in these coatings might effectively reduce wear acting as localized regions accumulating wear debris. The result shows that wear rate of all the coatings are lower as compared to MDN 321 substrate at all the test conditions. NiCrAlY/WC-Co/Cenosphere/MoS2/CaF2 and NiCrAlY/WC-Co/Cenosphere/MoS/CaSO4 coatings registered lower friction coefficient as compared to NiCrAlY/WC-Co/Cenosphere coating and MDN 321 substrate. Characterization of the NiCrAlY/WC-Co/Cenosphere/MoS2/CaF2 and NiCrAlY/WC-Co/Cenosphere/MoS2/CaSO4 coatings worn out surface suggests that MoS2 provides lubrication at 200 °C and formation of CaMoO4, MoO3 through tribo chemistry reaction at higher temperature provides lubrication at 600 °C. SEM micrograph of worn surface demonstrates that the main wear mechanism is plowing and delamination. © 2018 Elsevier B.V.
  • Item
    Plasma sprayed Cr3C2-NiCr/fly ash cenosphere coating: Cyclic oxidation behavior at elevated temperature
    (Institute of Physics Publishing helen.craven@iop.org, 2018) Doddamani, M.; Mathapati, M.; Ramesh, M.R.
    Oxidation is one of the major degradation phenomena observed in components subjected to higher temperatures like in thermal power plants (boiler tubes), steam and gas turbines blades etc. Developing protective coatings for such components mitigate oxidation. In the present study, plasma spray technique is utilized to deposit the Cr3C2-NiCr/Cenospheres coating on MDN 321 steel substrate. Thermo cyclic oxidation test is conducted at 600 °C (20 cycles) on both the coating and MDN 321 steel substrate. The thermogravimetric methodology is employed to estimate the oxidation kinetics. Energy Dispersive Spectroscopy (EDS), x-ray Diffraction (XRD), Scanning Electron Microscope (SEM) and x-ray mapping technique is employed to characterize the oxidized samples. Cr3C2-NiCr/Cenosphere coating displayed lower rate of oxidation as compared to substrate implying its suitability in high-temperature applications. Protective oxides like Al2O3, Cr2O3, and NiCr2O4 are observed on the uppermost layer of the coating lowering the oxidation rate in the developed coating. © 2018 IOP Publishing Ltd.